性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 |
基本性能 | 密度 | | ASTM D-1505 | 0.948 | g/cm3 |
熔体流动速率 | 190℃/21.6kg | ASTM D-1238 | 10 | g/10min |
薄膜厚度-Tested | | | 12.5 | um |
机械性能 | 环境应力开裂 | 50℃,100% Igepal,Compression Molded,F50 | ASTM D-1693 | >1000 | hr |
拉伸模量-1% Secant | Compression Molded | ASTM D-638 | 537 | MPa |
拉伸屈服强度 | Compression Molded | ASTM D-638 | 25 | MPa |
拉伸断裂强度 | Compression Molded | ASTM D-638 | 27 | MPa |
拉伸断裂伸长率 | Compression Molded | ASTM D-638 | 1300 | % |
拉伸屈服伸长率 | Compression Molded | ASTM D-638 | 10 | % |
弯曲模量 | Compression Molded | ASTM D-790 | 963 | MPa |
割线模量-1% Secant | 12.5um,Blown Film | ASTM D-882 | | MPa |
拉伸屈服强度 | 12.5um,Blown Film | ASTM D-882 | | MPa |
拉伸断裂强度 | 12.5um,Blown Film | ASTM D-882 | | MPa |
拉伸屈服伸长率 | 12.5um,Blown Film | ASTM D-882 | | % |
拉伸断裂伸长率 | 12.5um,Blown Film | ASTM D-882 | | % |
落锤冲击 | 12.5um,Blown Film | ASTM D-1709A | 140 | g |
IZOD缺口冲击强度 | Compression Molded | ASTM D-256 | 224 | J/m |
邵氏硬度 | Shore D,Compression Molded | ASTM D-2240 | 61 | |
热性能 | 热变形温度 | 0.45MPa,Unannealed,Compression Molded | ASTM D-648 | 60 | ℃ |
维卡软化点 | | ASTM D-1525 | 125 | ℃ |